| 560 | 10 | 82 |
| 下载次数 | 被引频次 | 阅读次数 |
通过测定导电剂的吸水能力,研究了导电剂的振实密度与吸液能力的关系,结果表明:导电剂的振实密度越大,其吸液能力越小;反之亦然。利用充放电性能曲线、循环伏安法和电化学阻抗法研究了GD、SP、KS、SO四种导电剂单一和两两混合使用作为锂离子电池正极LiCoO2导电剂时的电极性能。结果表明:SO和GD的混合物为导电剂时LiCoO2电极的性能最好,首次放电容量为141.4mAh·g-1。
Abstract:The relationship between the tap density and the liquid absorbili ty of the conductive agents was studied .The results showed the liquid absorbility decreased with increasing of its tap density. The effects of the single conduct ive agents and binary conductive agents consisting four kinds of carbon particle s with different sizes in a LiCoO2 cathode on the performance of lithium ion sec ondary batteries were reported. The performance was studied by various electroch emical methods, e.g., charge- discharge curves, A C impeda- nce technique and cyclic voltammetry curves.The results showed that the batte ry properties were better when the conductive agents were SO+ GD,and the first discharge capacity reached 141.4mAh· g- 1.
[1]宋文顺.化学电源工艺学[M].北京:中国轻工业出版社,1998.
[2]G uyom ard D,Tarascon J M.R echargeable Li1+x M n2O4/carbon cells loith a new electrolyte com position.Potentiostatic studies and application to practical cells[J].J Electrochem Soc,1993,140(11):3071-3075.
[3]C heon S E,K w on C W,K im D B,etal.Effectofbinary conductive agents in LiCoO2cathode on perform ances ofLithium ion polym er battery[J].J E lectrochim A cta,2000,46(8):599-605.
[4]Sato Y,M iyagi H,Takano H,et al.Transit-tim e-lim ited shot noise due to carriergeneration in sem iconductors:A new approach[J].Solid-State Electronics,1998,42(4):664-666.
基本信息:
中图分类号:TM912
引用信息:
[1]王力臻,王红芳,谷书华,任海中,李继春,李荣富,袁中平,苑永.导电剂对锂离子电池正极性能的影响[J].电池工业,2005(05):.
2005-10-25