| 163 | 0 | 230 |
| 下载次数 | 被引频次 | 阅读次数 |
锂离子电池无钴正极材料的开发对降低成本和提升安全性至关重要,但传统镍锰(Ni-Mn)体系因结构失稳和动力学性能不足面临挑战。本研究提出通过高熵协同掺杂(HignEntropyDoping,简称HE)与快离子导体界面工程的双重策略,构建高性能无钴镍锰正极材料(LiNi0.75Mn0.2Mg0.01Al0.01Zr0.01Ti0.01Mo0.01O2)。采用多元金属(Mg/Al/Zr/Ti/Mo)共掺杂形成高熵无序固溶体,显著抑制阳离子混排(Ni2+/Li+混排度由4.01%降至3.27%),并通过LiNbO3或 Li1.3Al0.3Ti1.7(PO4)3包覆优化界面锂离子传输动力学。结果表明:表面包覆材料(HE+LNO、HE+LATP)在0.1C下比容量达到194.1 mAh/g,2C倍率容量保持率88.2%,100次循环后容量保持率>95%,电荷转移电阻(Rct)较未包覆样品降低54%~56%。同时,高熵掺杂将热失控起始温度提升至248.9℃,放热量较初始未掺杂包覆样品减少~15%。该研究为无钴正极材料的设计提供了“体相-界面”协同优化新范式,兼具高容量、长循环寿命与优异热安全性。
Abstract:The development of cobalt-free positive terminal materials for lithium-ion batteries is crucial for reducing costs and improving safety, but traditional nickel-manganese (Ni-Mn) systems face challenges due to structural instability and insufficient kinetics. This study proposes a dual strategy of high entropy collaborative doping and fast ion conductor interfacial engineering to construct high-performance cobalt-free positive terminal materials (LiNi0.75Mn0.2Mg0.01Al0.01Zr0.01Ti0.01Mo0.01O2). Using multimetallic codoping (Mg/Al/Zr/Ti/Mo) to form high entropy disordered solid solutions significantly suppresses cathode mixing (Ni2+/Li+ mixing degree decreased from 4.01% to 3.27%), and optimizes interfacial lithium-ion transport kinetics through LiNbO3 or Li1.3Al0.3Ti1.7(PO4)3 enveloping. The results showed that surface coated materials (HE+LNO, HE+LATP) achieved a specific capacity of 194.1 mAh/g at 0.1C, a 2C capacity retention rate of 88.2%, a capacity retention rate of >95% after 100 cycles, and a charge transfer resistance (Rct) reduced by 54–56% compared to uncoated samples. At the same time, high entropy doping increased the initial thermal runaway temperature to 248.9℃, and the heat release was reduced by ~15% compared to initial uncoated samples. The study provided a new paradigm of "solid phase-interfacial collaborative optimization" for the design of cobalt-free positive terminal materials, combining high capacity, long cycle life, and superior thermal safety.
[1] LIM B B,YOON S J,PARK K J,et al.Advanced concentration gradient cathode material with two-slope for high-energy and safe lithium batteries[J].Advanced Functional Materials,2015,25(29):4673-4680.
[2] LIU W,OH P,LIU X E,et al.Nickel-rich layered lithium transition-metal oxide for high-energy lithium-ion batteries[J].Angewandte Chemie International Edition,2015,54(15):4440-4457.
[3] MURALIDHARAN N,SELF E C,DIXIT M,et al.Next-generation cobalt-free cathodes–a prospective solution to the battery industry’s cobalt problem[J].Advanced Energy Materials,2022,12(9):2103050.
[4] YOON W S,GREY C P,BALASUBRAMANIAN M,et al.In situ X-ray absorption spectroscopic study on LiNi_(0.5)Mn_(0.5)O_(2) cathode material during electrochemical cycling[J].Chemistry of Materials,2003,15(16):3161-3169.
[5] SUN Y K,LEE D J,LEE Y J,et al.Cobalt-free nickel rich layered oxide cathodes for lithium-ion batteries[J].ACS Applied Materials & Interfaces,2013,5(21):11434-11440.
[6] KO S,LEE S C,LEE C W,et al.A co-free layered LiNi_(0.7)Mn_(0.3)O_(2) cathode material for high-energy and long-life lithium-ion batteries[J].Journal of Alloys and Compounds,2014,613:96-101.
[7] PARK G T,NAMKOONG B,KIM S B,et al.Introducing high-valence elements into cobalt-free layered cathodes for practical lithium-ion batteries[J].Nature Energy,2022,7(10):946-954.
[8] CHOI S,FENG W L,XIA Y Y.High entropy and co-free high nickel based layered LiNi_(0.9)Mn_(0.1)O_(2) cathode for Li-ion batteries[J].ACS Applied Energy Materials,2024,7(8):3339-3346.
[9] LIANG L W,SU M S,SUN Z F,et al.High-entropy doping promising ultrahigh-Ni co-free single-crystalline cathode toward commercializable high-energy lithium-ion batteries[J].Science Advances,2024,10(25):eado4472.
[10] NIE Y,XIAO W,MIAO C,et al.Boosting the electrochemical performance of LiNi_(0.8)Co_(0.15)Al_(0.05)O_(2) cathode materials in-situ modified with Li_(1.3)Al_(0.3)Ti_(1.7)(PO4)_(3) fast ion conductor for lithium-ion batteries[J].Electrochimica Acta,2020,353:136477.
[11] LI Z,YOU Y,LIU Y,et al.Analyzing the mechanism of performance improvement in LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2) through coating with LiNbO_(3) fast ion conductor[J].Ceramics International,2024,50(17):30493-30503.
[12] LU G Z,PENG W X,ZHANG Y T,et al.Study on the formation,development and coating mechanism of new phases on interface in LiNbO_(3)-coated LiCoO_(2)[J].Electrochimica Acta,2021,368:137639.
[13] YU H F,WANG S L,HU Y J,et al.Lithium-conductive LiNbO_(3) coated high-voltage LiNi_(0.5)Co_(0.2)Mn_(0.3)O_(2) cathode with enhanced rate and cyclability[J].Green Energy & Environment,2022,7(2):266-274.
[14]SUN Q,CHEN X,XIE J,et al. Nano-Structured Li1.3al0.3ti1.7(Po4)3 Coated Licoo2 Enabling Compatible Interface with Ultrathin Garnet-Based Solid Electrolyte for Stable Li Metal Battery[J].Materials Today Nano,2022,8(19):100235.
[15] SUN Z,LAI Y Q,LV N,et al.Boosting the electrochemical performance of all-solid-state batteries with sulfide Li_(6)PS_(5)Cl solid electrolyte using Li_(2)WO_(4)-coated LiCoO_(2) cathode[J].Advanced Materials Interfaces,2021,8(15):2100624.
[16] YU J,PENG J X,HUANG W L,et al.Inhibition of excessive SEI-forming and improvement of structure stability for LiNi_(0.8)Co_(0.1)Mn_(0.1)O_(2) by Li_(2)MoO_(4) coating[J].Ionics,2021,27(7):2867-2876.
基本信息:
中图分类号:O646;TM912
引用信息:
[1]尹翔,李双福,杨明轩.高熵协同与界面工程驱动的无钴镍锰正极材料[J].电池工业().
基金信息:
国家重点研发计划,新能源汽车专项:无钴动力电池及梯次应用技术(2022YFB2502300)
2026-03-23
2026-03-23
2026-03-23