从普通锌锰电池及碱性锌锰电池中汞含量的现状和无汞化技术现状着手,分析了锌锰电池今后的发展取向。详细讨论了国内外相关电池法规中有关锌锰电池的部分;国内外,都禁止向电池中添加汞、镉、铅等有害元素。锌锰电池中的糊式电池的生存空间将会越来越小,锌锰电池将向无汞碱性锌锰电池的方向发展。
Abstract:The future developing trend of common zinc-managanese dioxide battery was analyzed through the mercury-free technology status and Hg content status of the zinc-managanese dioxide battery and alkaline zinc-managanese dioxide battery.And parts of relative rules and laws on the batteries both here and abroad were discussed in detail.It's forbidden to add harmful element such as Hg,Cd and Pb in battery at home and abroad.The survival space of the paste zinc-manganese dioxide battery would become smaller and smaller.The zinc-managanese dioxide battery would develop to the mercury-free alkaline zinc-managanese dioxide battery.
[1]环网.废旧电池回收何日走出尴尬[J].中国资源综合利用,2002,8:44.
[2]王金良,马扣祥.也谈废电池的回收利用[J].电池工业,2000,5(6):267-271.
[3]王金良,王淇.再谈废电池的污染及防治[J].电池工业,2003,8(1):37-40.
[4]聂永丰.废电池的危害及其环境污染风险分析[J].节能与环保,2004,2:5-6.
[5]武德俊.聚焦废电池污染防治[J].节能与环保,2004,2:1-4.
[6]国家环保局.环发[2003〗163号,废电池污染防治技术政策[J].2003-10-9
[7]中国轻工总会.轻总行管[1997]4号,关于限制电池产品汞含量的规定[J].1997-12-31.
[8]刘煦,宋园园,邱仕洲.锌锰电池无害化发展探讨[J].电池工业,2003,8(4):185-188.
[9]王金良.欧盟修改电池指令对我国电池行业的影响[J].电池工业,2003,8(5):232-235.
[10]钱敦勇.国产设备生产无汞碱锰电池[J].电池工业,2001,6(5):214-216.
[11]白永兰,李伟善,黎凤鸣,等.碱性锌锰电池负极锌粉缓蚀剂[J].电池工业,2002,7(3-4):116-120.
[12]王金良,王益波,孟波,等.无汞碱性锌锰电池的研制[J].电池工业,1998,3(4):101-106.
[13]王力臻.碱性锌锰电池无汞化中的若干问题[J].电池工业,1998,3(5):148-152.
[14]王金良.再谈碱性锌锰电池的无汞化[J].电池工业,2000,5(3):99-104.
[15]李诚芳.汞在碱性锌锰电池中的作用及去汞措施[J].电池工业,2001,6(4):150-152.
[16]何永基.无水银碱性钮形电池[P].中国专利:ZL01234722.1,2002-10-02.
[17]国家环境保护总局科技标准司.废电池污染防治技术政策编制说明[J].2002-12.
[18]曹国庆,沈英娃,菅小东.废旧电池管理与环保法规[J].电池工业,2002,7(6):322-325.
[19]http://www.baj.or.jp/about/enviprogram.htm l.
[20]EC.Council D irective 91/157/EEC.O n batteries and ac-cum ulators containing certain dangerous substances[Z].1991-03-18.
基本信息:
中图分类号:X321;F426.6
引用信息:
[1]马扣祥.锌锰电池的污染与产业政策[J].电池工业,2006(05):338-341.
2006-10-25
2006-10-25